Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 28.811 MPa @Strain 2.20 %, Temperature 150 °C |
4178.7 psi @Strain 2.20 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |