Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.96 MPa @Strain 100 % |
284 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P2855B TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.96 MPa @Strain 300 % |
284 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3740 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.96 MPa @Strain 300 % |
284 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P52-004A-3B TPE, PP Overmold or Standalone use Characteristics: Soft, flexible feelExcellent grip characteristicsGood weatherabilityGood compression setEasy processability and colorabilityAvailable FDA and medical gradesAvailable translucent gra.. |
|||
Tensile Stress | 1.96 MPa @Strain 300 % |
284 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P1935 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |