Polymer Property : Tensile Stress = 2870 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 19.8 MPa

@Strain 2.00 %,
Temperature 80.0 °C
2870 psi

@Strain 2.00 %,
Temperature 176 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D..
Tensile Stress 19.8 MPa

@Strain 0.140 %,
Temperature 23.0 °C
2870 psi

@Strain 0.140 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA)
35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e..
Tensile Stress 19.79 MPa

@Strain 0.460 %,
Temperature 90.0 °C
2870 psi

@Strain 0.460 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610
30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Zytel RS 30G30L NC010 is a lubricated 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewabl..
Tensile Stress 19.8 MPa

@Strain 1.90 %,
Temperature 90.0 °C
2870 psi

@Strain 1.90 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical ..
Tensile Stress 19.8 MPa

@Strain 0.250 %,
Temperature -40.0 °C
2870 psi

@Strain 0.250 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. ..