Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.07 MPa @Strain 100 % |
445 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® A9760 TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Stress | 3.07 MPa @Strain 48.12 %, Temperature 120 °C |
445 psi @Strain 48.12 %, Temperature 248 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**) Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject.. |
|||
Tensile Stress | 3.07 MPa @Strain 5.62 %, Temperature 60.0 °C |
445 psi @Strain 5.62 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET
(Unverified Data**) 44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin.. |