Mechanical Properties Metric English Comments
Tensile Stress 31.0 MPa

@Strain 3.80 %,
Temperature 40.0 °C
4500 psi

@Strain 3.80 %,
Temperature 104 °F
ISO 527
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers
Tensile Stress 31.0 MPa

@Strain 0.180 %,
Temperature 23.0 °C
4500 psi

@Strain 0.180 %,
Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Rynite® FR543 NC010 PET
Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm..
Tensile Stress 31.0 MPa

@Strain 4.58 %,
Temperature 180 °C
4500 psi

@Strain 4.58 %,
Temperature 356 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66  (Unverified Data**)
20% Glass Reinforced Heat Stabilized Polyamide 66 Developed for Blow Molding Zytel BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Perf..
Tensile Stress 31.0 MPa

@Strain 300 %
4500 psi

@Strain 300 %
ASTM D412
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Zythane™ 3045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 31.0 MPa

@Strain 0.600 %,
Time 3.60e+6 sec
4500 psi

@Strain 0.600 %,
Time 1000 hour
ISO 899-1
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM
Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness.
Tensile Stress 31.0 MPa

@Time 3600 sec,
Strain 2.00 %
4500 psi

@Time 1.00 hour,
Strain 2.00 %
ISO 899-1
BASF Ultraform N 2320 003 UNC Q600 POM
Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent.
Tensile Stress 31.0 MPa

@# of Cycles 1.00e+7 ,
Temperature 180 °C
4500 psi

@# of Cycles 1.00e+7 ,
Temperature 356 °F
BASF Ultrason E 2010 G6 30% Glass Filled PES
Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength.
Tensile Stress 31.0 MPa

@Strain 50.0 %,
Temperature 100 °C
4500 psi

@Strain 50.0 %,
Temperature 212 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66  (Unverified Data**)
Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi..
Tensile Stress 31.0 MPa

@Strain 1.56 %,
Temperature 60.0 °C
4500 psi

@Strain 1.56 %,
Temperature 140 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT  (Unverified Data**)
Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..