Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.15 MPa @Strain 100 % |
312 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® A9845 TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Stress | 2.15 MPa @Strain 100 % |
312 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® A9960 TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Stress | 2.15 MPa @Strain 100 % |
312 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® A9960C TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Stress | 2.15 MPa @Strain 100 % |
312 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® A9970H TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Stress | 2.15 MPa @Strain 300 % |
312 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® C4640 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Stress | 2.15 MPa @Strain 100 % |
312 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P2945T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.15 MPa @Strain 9.12 %, Temperature 100 °C |
312 psi @Strain 9.12 %, Temperature 212 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**) Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject.. |
|||
Tensile Stress | 2.15 MPa @Strain 92.53 %, Temperature 200 °C |
312 psi @Strain 92.53 %, Temperature 392 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |