Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 21.67 MPa @Strain 1.00 %, Temperature 90.0 °C |
3143 psi @Strain 1.00 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 79G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Polyamide 66 Zytel 79G13L NC010 is a 13% glass fiber reinforced toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 21.67 MPa @Strain 26.87 %, Temperature 40.0 °C |
3143 psi @Strain 26.87 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC4601 NC010 Nylon
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide Developed for Extrusion Zytel RS LC4601 NC010 is a flexible toughened and plasticized polyamide resin intended for extrusion applications.Informatio.. |