Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.24 MPa @Strain 100 % |
325 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® A9860M TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Stress | 2.24 MPa @Strain 100 % |
325 psi @Strain 100 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ EG-9065 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun.. |
|||
Tensile Stress | 2.24 MPa @Strain 50.0 % |
325 psi @Strain 50.0 % |
ASTM D412 Method A |
Seals Eastern 7346 Extreme Low Temperature Service Rubber HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern. |
|||
Tensile Stress | 2.24 MPa @Strain 0.100 %, Temperature 23.0 °C |
325 psi @Strain 0.100 %, Temperature 73.4 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |