Mechanical Properties Metric English Comments
Tensile Stress 33.0 MPa

@Strain 10.0 %,
Temperature 60.0 °C
4790 psi

@Strain 10.0 %,
Temperature 140 °F
ISO 527
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers
Tensile Stress 33.0 MPa

@Strain 1.30 %,
Temperature -40.0 °C
4790 psi

@Strain 1.30 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)  (Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri..
Tensile Stress 33.0 MPa

@Strain 4.80 %,
Temperature 90.0 °C
4790 psi

@Strain 4.80 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..
Tensile Stress 33.0 MPa

@Strain 0.700 %,
Temperature -40.0 °C
4790 psi

@Strain 0.700 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..
Tensile Stress >= 33.0 MPa

@Strain 300 %
>= 4790 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 264D Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tensile Stress 33.0 MPa

@Strain 50.0 %,
Temperature 80.0 °C
4790 psi

@Strain 50.0 %,
Temperature 176 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66  (Unverified Data**)
Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi..
Tensile Stress 33.0 MPa

@Strain 50.0 %,
Temperature 100 °C
4790 psi

@Strain 50.0 %,
Temperature 212 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66  (Unverified Data**)
Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi..