Mechanical Properties Metric English Comments
Tensile Stress 2.31 MPa

@Strain 300 %
335 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® D6840 TPE, Extruded
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from..
Tensile Stress 2.31 MPa

@Strain 300 %,
Temperature 23.0 °C
335 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ 9555-1 Thermoplastic Elastomer (TPE)
Versaflex™ 9555-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Tensile Stress 2.31 MPa

@Strain 300 %,
Temperature 23.0 °C
335 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ 9555-9 Thermoplastic Elastomer (TPE)
Versaflex™ 9555-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to ..
Tensile Stress 2.31 MPa

@Strain 300 %,
Temperature 23.0 °C
335 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versalloy™ HC 9210-55N Thermoplastic Elastomer (TPE)
Versalloy™ HC 9210-55N is a TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgical grips. Prod..
Tensile Stress 2.31 MPa

@Strain 300 %,
Temperature 23.0 °C
335 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versalloy™ XL 9055-1 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9055-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov..
Tensile Stress 2.31 MPa

@Strain 300 %,
Temperature 23.0 °C
335 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versalloy™ XL 9055X-9 Thermoplastic Elastomer (TPE)
Versalloy™ XL 9055X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Overmold Adhesion to Polypro..
Tensile Stress 2.31 MPa

@Strain 300 %
335 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P3857CT TPE, PP Overmold or Standalone use