Polymer Property : Tensile Stress = 34.07 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 34.07 MPa

@Strain 0.300 %,
Temperature 0.000 °C
4941 psi

@Strain 0.300 %,
Temperature 32.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610  (Unverified Data**)
20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers