Mechanical Properties Metric English Comments
Tensile Stress 34.16 MPa

@Strain 1.05 %,
Temperature 150 °C
4954 psi

@Strain 1.05 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po..
Tensile Stress 34.16 MPa

@Strain 0.230 %,
Temperature 0.000 °C
4954 psi

@Strain 0.230 %,
Temperature 32.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612  (Unverified Data**)
43% Glass Reinforced Polyamide 612Zytel 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers