Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 235 MPa @Strain 2.00 %, Temperature 23.0 °C |
34100 psi @Strain 2.00 %, Temperature 73.4 °F |
|
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |