Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 35.6 MPa @Strain 18.0 %, Temperature 60.0 °C |
5160 psi @Strain 18.0 %, Temperature 140 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |