Mechanical Properties Metric English Comments
Tensile Stress 37.1 MPa

@Strain 1.99 %,
Temperature 150 °C
5380 psi

@Strain 1.99 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)  (Unverified Data**)
40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te..
Tensile Stress 37.1 MPa

@Strain 0.280 %,
Temperature 90.0 °C
5380 psi

@Strain 0.280 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G45HSL NC010 Polyphthalamide (PPA)  (Unverified Data**)
45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL NC010 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..