Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 25.66 MPa @Strain 0.250 %, Temperature 40.0 °C |
3722 psi @Strain 0.250 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR NC010 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |