Polymer Property : Tensile Stress = 38.74 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 38.74 MPa

@Strain 2.48 %,
Temperature 90.0 °C
5619 psi

@Strain 2.48 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)  (Unverified Data**)
35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de..
Tensile Stress 38.74 MPa

@Strain 1.45 %,
Temperature -40.0 °C
5619 psi

@Strain 1.45 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66  (Unverified Data**)
Toughened Heat Stabilized Polyamide 66 Zytel 444AHS is a toughened heat stabilized black polyamide 66 resin for injection molding. It is a high flow processing friendly material.Information provided..