Mechanical Properties Metric English Comments
Tensile Stress 26.6 MPa

@Strain 0.700 %,
Temperature 0.000 °C
3860 psi

@Strain 0.700 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..