Mechanical Properties Metric English Comments
Tensile Stress 2.73 MPa

@Strain 300 %
396 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P1865A TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.73 MPa

@Strain 300 %
396 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P3950CT TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 2.73 MPa

@Strain 0.110 %,
Temperature 23.0 °C
396 psi

@Strain 0.110 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)  (Unverified Data**)
Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also..
Tensile Stress 2.73 MPa

@Strain 6.28 %,
Temperature 0.000 °C
396 psi

@Strain 6.28 %,
Temperature 32.0 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers