Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.09 MPa @Strain 100 % |
593 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® F02-087B TPE, Halogen Free Extrusion Grade Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to.. |