Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.82 MPa @Strain 100 % |
699 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3975H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 4.82 MPa @Strain 10.44 %, Temperature 150 °C |
699 psi @Strain 10.44 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC4601 NC010 Nylon
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide Developed for Extrusion Zytel RS LC4601 NC010 is a flexible toughened and plasticized polyamide resin intended for extrusion applications.Informatio.. |