Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 42.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 42.0 MPa

@Strain 9.50 %,
Temperature 40.0 °C
6090 psi

@Strain 9.50 %,
Temperature 104 °F
ISO 527
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers
Tensile Stress 42.0 MPa

@Strain 12.0 %,
Temperature 120 °C
6090 psi

@Strain 12.0 %,
Temperature 248 °F
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY
Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th..
Tensile Stress 42.0 MPa

@Strain 1.00 %
6090 psi

@Strain 1.00 %
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, Conditioned
Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers..
Tensile Stress 42.0 MPa

@Strain 30.0 %,
Temperature 80.0 °C
6090 psi

@Strain 30.0 %,
Temperature 176 °F
Solvay TECHNYL® A 205F PA66, DRY
Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities..
Tensile Stress 42.0 MPa

@Strain 2.40 %,
Temperature 23.0 °C
6090 psi

@Strain 2.40 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani..
Tensile Stress 42.0 MPa

@Strain 2.40 %,
Temperature 23.0 °C
6090 psi

@Strain 2.40 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b..
Tensile Stress 42.0 MPa

@Strain 1.80 %,
Temperature 150 °C
6090 psi

@Strain 1.80 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
Tensile Stress 42.0 MPa

@Strain 1.22 %,
Temperature 90.0 °C
6090 psi

@Strain 1.22 %,
Temperature 194 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66
Information provided by DuPont Performance Polymers
Tensile Stress 42.0 MPa

@Strain 100 %
6090 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 6065D Thermoplastic Polyurethane Elastomer
Zythane™ 6065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 42.0 MPa

@Strain 100 %
6090 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer
Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 42.0 MPa

@Strain 2.00 %,
Temperature 23.0 °C
6090 psi

@Strain 2.00 %,
Temperature 73.4 °F
ISO 527
BASF Ultrason E 3010 PES
Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance.
Tensile Stress >= 42.0 MPa

@Strain 300 %
>= 6090 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 472D Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Stress >= 42.0 MPa

@Strain 300 %
>= 6090 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 672D Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Stress 42.0 MPa

@Strain 4.00 %,
Temperature 30.0 °C
6090 psi

@Strain 4.00 %,
Temperature 86.0 °F
ISO 527
BASF Ultradur B 4520 PBT
Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade.
Copyright © lookpolymers.com All Rights Reserved