Mechanical Properties Metric English Comments
Tensile Stress 0.290 MPa

@Strain 0.0300 %,
Temperature -20.0 °C
42.1 psi

@Strain 0.0300 %,
Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610  (Unverified Data**)
Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie..