Mechanical Properties Metric English Comments
Tensile Stress 42.21 MPa

@Strain 2.90 %,
Temperature 100 °C
6122 psi

@Strain 2.90 %,
Temperature 212 °F
ISO 11403-1/-2
DuPont Performance Polymers Crastin® LW9330 BK851 PBT  (Unverified Data**)
Crastin® LW9330 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp..
Tensile Stress 42.21 MPa

@Strain 1.00 %,
Temperature 100 °C
6122 psi

@Strain 1.00 %,
Temperature 212 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66  (Unverified Data**)