Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 29.5 MPa @Strain 0.47291 %, Temperature -40.0 °C |
4280 psi @Strain 0.47291 %, Temperature -40.0 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 510GR NC000 Acetal Homopolymer
(Unverified Data**) Delrin® 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength, stiffness, and high deflection temperature and excellent creep resistance.Information provide.. |
|||
Tensile Stress | 29.5 MPa @Strain 6.16 %, Temperature 90.0 °C |
4280 psi @Strain 6.16 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66
(Unverified Data**) 30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |
|||
Tensile Stress | 29.51 MPa @Strain 20.0 %, Temperature 150 °C |
4280 psi @Strain 20.0 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info.. |
|||
Tensile Stress | 29.5 MPa @Strain 0.450 %, Temperature 40.0 °C |
4280 psi @Strain 0.450 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 29.5 MPa @Strain 0.620 %, Temperature 23.0 °C |
4280 psi @Strain 0.620 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |