Tensile Stress 29.6 MPa

@Strain 30.0 %,
Temperature 120 °C
4290 psi

@Strain 30.0 %,
Temperature 248 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66  (Unverified Data**)
Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers
Tensile Stress 29.6 MPa

@Strain 10.0 %,
Temperature 90.0 °C
4290 psi

@Strain 10.0 %,
Temperature 194 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66  (Unverified Data**)
Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers
Tensile Stress 29.6 MPa

@Strain 3.72 %,
Temperature 90.0 °C
4290 psi

@Strain 3.72 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66  (Unverified Data**)
30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa..