Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 43.2 MPa @Strain 11.4 %, Temperature 40.0 °C |
6270 psi @Strain 11.4 %, Temperature 104 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |