Polymer Property : Tensile Stress = 4328 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 29.84 MPa

@Strain 2.07 %,
Temperature 150 °C
4328 psi

@Strain 2.07 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 79G13L NC010 Nylon 66  (Unverified Data**)
13% Glass Reinforced Toughened Polyamide 66 Zytel 79G13L NC010 is a 13% glass fiber reinforced toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers