Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 44.88 MPa @Strain 1.15 %, Temperature 90.0 °C |
6509 psi @Strain 1.15 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR70G25V0 NC010 is a 25% glass fiber reinforced heat stabilized flame retardant polyamide 66 resin for injection molding.Information provided .. |