Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 45.1 MPa @Strain 2.91 %, Temperature 150 °C |
6540 psi @Strain 2.91 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK549 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 45.1 MPa @Strain 1.56 %, Temperature 90.0 °C |
6540 psi @Strain 1.56 %, Temperature 194 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |