Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 32.99 MPa @Strain 0.340 %, Temperature 40.0 °C |
4785 psi @Strain 0.340 %, Temperature 104 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK608 BK509 PBT
(Unverified Data**) Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 32.99 MPa @Strain 0.590 %, Temperature 180 °C |
4785 psi @Strain 0.590 %, Temperature 356 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |