Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 33.03 MPa @Strain 12.0 %, Temperature 90.0 °C |
4791 psi @Strain 12.0 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6
(Unverified Data**) 30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |