Mechanical Properties Metric English Comments
Tensile Stress 3.31 MPa

@Strain 300 %,
Temperature 23.0 °C
480 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ HC MT555 Thermoplastic Elastomer (TPE)
Versaflex™ HC MT555 is an easy processing material designed for applications where FDA compliance and medical testing is required. - Excellent Colorability - Soft TouchRear: 340 - 360F Center: 380 ..
Tensile Stress 3.31 MPa

@Strain 100 %,
Temperature 23.0 °C
480 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 6275-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6275-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. New Prod..
Tensile Stress 3.31 MPa

@Strain 100 %
480 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® D6965H TPE, Extruded
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from..
Tensile Stress >= 3.31 MPa

@Strain 50.0 %
>= 480 psi

@Strain 50.0 %
ASTM D412 Method A
Seals Eastern 7352D Nano-PTFE Filled Fluoroelastomer
Nano-PTFE filled fluoroelastomer for low wear in hot dynamic applicationsInformation provided by Seals Eastern.
Tensile Stress 3.31 MPa

@Strain 300 %
480 psi

@Strain 300 %
ASTM D412
Teknor Apex Telcar® TL-1050-75 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Stress 3.31 MPa

@Strain 300 %
480 psi

@Strain 300 %
ASTM D412
Teknor Apex Telcar® TL-1520C Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Stress 3.31 MPa

@Strain 98.33 %,
Temperature 120 °C
480 psi

@Strain 98.33 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers