Tensile Stress 33.3 MPa

@Strain 1.10 %,
Temperature -40.0 °C
4830 psi

@Strain 1.10 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 520MP NC010 Acetal (POM)  (Unverified Data**)
20% Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 520MP is a medium viscosity acetal homopolymer containing 20% Teflon PTFE Micropowder. It is designe..
Tensile Stress 33.3 MPa

@Strain 27.0 %,
Temperature 90.0 °C
4830 psi

@Strain 27.0 %,
Temperature 194 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66  (Unverified Data**)
Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers
Tensile Stress 33.3 MPa

@Strain 0.600 %,
Temperature 23.0 °C
4830 psi

@Strain 0.600 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 11C40 NC010 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66 Minlon 11C40 NC010 is a 40% mineral reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers