Polymer Property : Tensile Stress = 4973 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 34.29 MPa

@Strain 4.13 %,
Temperature 150 °C
4973 psi

@Strain 4.13 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen..