Mechanical Properties Metric English Comments
Tensile Stress 5.17 MPa

@Strain 300 %
750 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ EG-9177 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun..
Tensile Stress 5.17 MPa

@Strain 300 %
750 psi

@Strain 300 %
ASTM D412
Teknor Apex Telcar® TL-1025-75 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Stress 5.17 MPa

@Strain 0.0600 %,
Temperature 150 °C
750 psi

@Strain 0.0600 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)  (Unverified Data**)
60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo..
Tensile Stress 5.17 MPa

@Strain 0.0500 %,
Temperature 120 °C
750 psi

@Strain 0.0500 %,
Temperature 248 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..