Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.72 MPa @Strain 300 % |
830 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3880H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 5.72 MPa @Strain 0.0400 %, Temperature 40.0 °C |
830 psi @Strain 0.0400 %, Temperature 104 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66
(Unverified Data**) Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in.. |