Mechanical Properties Metric English Comments
Tensile Stress 5.81 MPa

@Strain 300 %,
Temperature 23.0 °C
843 psi

@Strain 300 %,
Temperature 73.4 °F
Die C Flow 2 hr; ASTM D412
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE)
Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr..
Tensile Stress 5.81 MPa

@Strain 7.64 %,
Temperature 150 °C
843 psi

@Strain 7.64 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo..