Mechanical Properties Metric English Comments
Tensile Stress 34.55 MPa

@Strain 0.790 %,
Temperature 90.0 °C
5011 psi

@Strain 0.790 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET)
20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol..