Mechanical Properties Metric English Comments
Tensile Stress 34.76 MPa

@Strain 2.48 %,
Temperature 90.0 °C
5042 psi

@Strain 2.48 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti..