Polymer Property : Tensile Stress = 52.32 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 52.32 MPa

@Strain 3.00 %,
Temperature 150 °C
7588 psi

@Strain 3.00 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66  (Unverified Data**)
33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provi..
Tensile Stress 52.32 MPa

@Strain 1.40 %,
Temperature 100 °C
7588 psi

@Strain 1.40 %,
Temperature 212 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G43HS1L BK104 is a 43% glass fiber reinforced, heat stabilized, black polyamide 66 resin with superior impact resistance.Information provided by DuPont Performance Polymers