Mechanical Properties Metric English Comments
Tensile Stress 52.86 MPa

@Strain 0.440 %,
Temperature 0.000 °C
7667 psi

@Strain 0.440 %,
Temperature 32.0 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA)
Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance ..