Tensile Stress 53.4 MPa

@Strain 4.80 %,
Temperature 40.0 °C
7750 psi

@Strain 4.80 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider..