Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 37.0 MPa @Strain 1.00 %, Temperature 100 °C |
5370 psi @Strain 1.00 %, Temperature 212 °F |
|
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim.. |
|||
Tensile Stress | >= 37.0 MPa @Strain 300 % |
>= 5370 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 464D Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | 37.0 MPa @Strain 50.0 %, Temperature 80.0 °C |
5370 psi @Strain 50.0 %, Temperature 176 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66
(Unverified Data**) Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi.. |