Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 54.9 MPa @Strain 25.9 %, Temperature -20.0 °C |
7960 psi @Strain 25.9 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Tensile Stress | 54.9 MPa @Strain 3.10 %, Temperature 23.0 °C |
7960 psi @Strain 3.10 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 300CP BK642 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc.. |
|||
Tensile Stress | 54.9 MPa @Strain 3.70 %, Temperature -20.0 °C |
7960 psi @Strain 3.70 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500AF Acetal (POM)
(Unverified Data**) 20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi.. |