Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 55.94 MPa @Strain 0.970 %, Temperature 40.0 °C |
8113 psi @Strain 0.970 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSLX BK357 is a 35% glass fiber reinforced heat stabilized black polyamide 66 for injection molding.Information provided by DuPont Perfor.. |
|||
Tensile Stress | 55.94 MPa @Strain 1.40 %, Temperature 150 °C |
8113 psi @Strain 1.40 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 51G45HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL NC010 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |