Mechanical Properties Metric English Comments
Tensile Stress 55.95 MPa

@Strain 7.24 %,
Temperature 150 °C
8115 psi

@Strain 7.24 %,
Temperature 302 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 53G50HSLR NC010 Polyphthalamide (PPA)  (Unverified Data**)
50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR NC010 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve..
Tensile Stress 55.95 MPa

@Strain 3.20 %,
Temperature 150 °C
8115 psi

@Strain 3.20 %,
Temperature 302 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G40DH1T BK261 Nylon  (Unverified Data**)
Zytel® PLS95G40DH1T is a 40% GR impact modified PA, made with SHIELD technology, its superior heat & oil resistance combined with the "stone impact resistance" makes it ideal choice for use in seve..