Mechanical Properties Metric English Comments
Tensile Stress 380 MPa

@Diameter 105 - 200 mm,
Strain 0.200 %
55100 psi

@Diameter 4.13 - 7.87 in,
Strain 0.200 %
United Cast Bar Unibar 700-2 Continuously Cast Spheroidal Graphite Iron
Offers higher wear resistance; strength & heat-treatment response while still possessing reasonable machinability and excellent surface finish. Noise and vibration damping are good in this grade.Uni..
Tensile Stress 380 MPa

@Diameter 205 - 600 mm,
Strain 0.200 %
55100 psi

@Diameter 8.07 - 23.6 in,
Strain 0.200 %
United Cast Bar Unibar 700-2 Continuously Cast Spheroidal Graphite Iron
Offers higher wear resistance; strength & heat-treatment response while still possessing reasonable machinability and excellent surface finish. Noise and vibration damping are good in this grade.Uni..