Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.82 MPa @Strain 100 % |
554 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3865B TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 3.82 MPa @Strain 37.24 %, Temperature 90.0 °C |
554 psi @Strain 37.24 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |