Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 57.7 MPa @Strain 2.30 %, Temperature -20.0 °C |
8370 psi @Strain 2.30 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Tensile Stress | 57.7 MPa @Strain 2.30 %, Temperature -20.0 °C |
8370 psi @Strain 2.30 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |
|||
Tensile Stress | 57.7 MPa @Strain 1.10 %, Temperature 0.000 °C |
8370 psi @Strain 1.10 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 57.7 MPa @Strain 0.720 %, Temperature 40.0 °C |
8370 psi @Strain 0.720 %, Temperature 104 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |